Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 17.3 - 17.7 g/cc | 0.625 - 0.639 lb/in³ | |
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Density | 17.3 - 17.7 g/cc | 0.625 - 0.639 lb/in³ | |
H.C. Starck HPM 1751 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |