Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.49 g/cc | 0.0900 lb/in³ | |
Schott NG1 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
Density | 2.49 g/cc | 0.0900 lb/in³ | |
Schott N-ZK7 Glass Information Provided by SCHOTT North America, Inc. |