Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Ferro IX 1944 Dental Glass Glass Type: Si-Al-Ca-F Typical Application: Glass-Ionomer Cement Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also man.. |
|||
Density | 2.71 g/cc | 0.0980 lb/in³ | |
IBC Advanced Alloys 2.6% BeAl Beryllium Aluminum Master Alloy Beryllium aluminum “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and.. |
|||
Density | 2.71 g/cc | 0.0980 lb/in³ | |
IBC Advanced Alloys 5% BeAl Beryllium Aluminum Master Alloy Beryllium aluminum “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
MarkeTech Calcium Carbonate, Calcite (CaCO3) Optical Grade Crystal Optical grade crystal with no small inclusions, cleavage planes, clouds and mist, point defects or bubbles inside the crystal. A proprietary process is used for cutting, grinding and polishing quali.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Lucas-Milhaupt AL 716 Aluminum Brazing Filler Metal Applications:AL 716 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa Excalibar® 6013-T8 Aluminum, 0.3-1.9 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa Excalibar® 6013-T8 Aluminum, 1.9-3.8 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa Excalibar® 6013-T8 Aluminum, 3.8-8.2 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa UltrAlloy® 6020-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa UltrAlloy® 6020-T9 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Alcoa Excalibar® 6013-T651 Aluminum Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. .. |
|||
Density | 2.71 g/cc | 0.0979 lb/in³ | |
Pyrotek Pyrocast ZA Refractory Shapes Aggregate Base: Mullite / SiCApplicationsWear Pads TCPT's Information provided by Pyrotek. |