Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 2.75 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.75 g/cc
0.0994 lb/in³
Ferro EG 2778 Thick Film Glass
Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..
Density 2.75 g/cc
0.0994 lb/in³
Apparent
Gouda Vuurvast AK 80 AP Dense Refractory Brick
Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks..
Density 2.75 g/cc
0.0994 lb/in³
Apparent
Gouda Vuurvast AK 80 B Dense Refractory Brick
Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr..
Density 2.75 g/cc
0.0994 lb/in³
Mateck Potassium Bromide (KBr)
Optical crystals
Density 2.75 g/cc
0.0994 lb/in³
Schott GG475 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG385, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Schott OG590 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, GG385, RG610, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Schott RG610 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, GG385, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Schott GG435 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG385, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Schott GG495 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG385, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Schott RG1000 Long Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630..
Density 2.75 g/cc
0.0994 lb/in³
Schott RG665 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Density 2.75 - 2.90 g/cc
0.0994 - 0.105 lb/in³
Tritex TRI-F Blanket Insulation
TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var..
Density 2.75 g/cc
0.0994 lb/in³
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Density 2.75 - 2.90 g/cc
0.0994 - 0.105 lb/in³
3M #11 Roofing Granule (Pittsboro)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..
Density 2.75 - 2.90 g/cc
0.0994 - 0.105 lb/in³
3M Headlap Roofing Granule (Pittsboro)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..
Density 2.75 g/cc
0.0994 lb/in³
Schott GG400 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG385, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Density 2.75 g/cc
0.0994 lb/in³
Indium Corp. Indalloy 189 Aluminum Solder Alloy
Information Provided by Indium Corporation