Polymer Property : Density = 2.77 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.780 - 2.77 g/cc
0.0282 - 0.100 lb/in³
Average value: 0.952 g/cc Grade Count:729
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..