Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.91 g/cc | 0.105 lb/in³ | |
Lucas-Milhaupt AL 719 Aluminum Brazing Filler Metal Applications:AL 719 filler metal is generally used to join aluminum and aluminum alloys. It has been used to join castings and otherwise unbrazeable aluminums. Care must be taken to be sure that t.. |
|||
Density | 2.91 g/cc @Temperature 25.0 °C |
0.105 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8651 Sealing Glass Tungsten sealing glass Power diodesInformation provided by SCHOTT AG. |
|||
Density | 2.91 g/cc | 0.105 lb/in³ | |
Schott N-PSK3 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.91 g/cc | 0.105 lb/in³ | |
Schott S8807 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Density | 2.91 g/cc | 0.105 lb/in³ | |
Schott S8808 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Density | 2.91 g/cc | 0.105 lb/in³ | |
Schott S8809 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |