Polymer Property : Density = 21.56 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 21.56 g/cc
0.7789 lb/in³
Goodfellow Platinum 90/Iridium 10 Alloy
The alloy has been used in "non-standard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.Information provided ..