Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.41 g/cc | 0.123 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 632 Mullite Brand 632 features: Light Weight Setter.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when th.. |