Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.87 g/cc | 0.140 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.87 g/cc | 0.140 lb/in³ | |
Anderman Ceramics EZZ 66P Zircon Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |