Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.88 g/cc | 0.140 lb/in³ | ISO 1183-1 |
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.Special Properties:• Lower sliding wear than Murflor®• Good slide properties• Low s.. |
|||
Density | 3.88 - 3.92 g/cc | 0.140 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9916 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.88 - 3.92 g/cc | 0.140 - 0.142 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | Sintered |
Nabaltec NABALOX® NO 613-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 55BZ+5Mos PTFE; Bronze/Molybdenum Disulphide Filled
(discontinued **) Data provided by the manufacturer.55 wt.% Bronze + 5 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properti.. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0388 Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0390 S1 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM-C373 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM-C373 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Density | 3.88 g/cc | 0.140 lb/in³ | ASTM-C373 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |