Polymer Property : Density = 4.27 g/cc
Polymer Property :
Density =
4.27 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
4.27
g/cc
0.154
lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system