Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.80 - 5.80 g/cc | 0.173 - 0.210 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr) |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | |
BASF Sicotan® Brown K 2711 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | A Component; ASTM D1475 |
Aptek 6516-A/B Electrically conductive epoxy adhesive General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of.. |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | B Component; ASTM D1475 |
Aptek 6516-A/B Electrically conductive epoxy adhesive General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of.. |