Polymer Property : Density = 4.89 g/cc
Polymer Property :
Density =
4.89 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
4.89
g/cc
0.177
lb/in³
MarkeTech Barium Fluoride, BaF2 Scintillator Crystal
Data provided by the supplier, MarkeTech International.