Polymer Property : Density = 5.75 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.75 g/cc
0.208 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 837 Zirconia + 4.4 mol% Calcia
Brand 837 features: Good spalling characteristics.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, ev..
Density 5.75 g/cc
0.208 lb/in³
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized
Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is ..
Density 5.75 g/cc
0.208 lb/in³
CoorsTek StatSafe™ ZDC Static Dissipative Zirconia
Specialized StatSafe™ ESD-safe zirconia combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffne..