Density
6.04
g/cc
0.218
lb/in³
without HIP; DIN EN 623-2
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade
MZ BE is a yttria-stabilized tetragonal zirconia used in dental applications.