Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.10 g/cc | 0.220 lb/in³ | |
MarkeTech Repton 838 Zirconia + 3 mol% Yttria (YSZ) Brand 838 features: Co-precipitation; high strength.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, .. |
|||
Density | 6.10 g/cc | 0.220 lb/in³ | |
MarkeTech Repton 848 Zirconia + 3 mol% Yttria (YSZ) REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 6.10 g/cc | 0.220 lb/in³ | |
MarkeTech Yttrium Aluminate (YAlO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
Density | 6.10 g/cc | 0.220 lb/in³ | |
MarkeTech Zirconium Oxide Ceramic Zirconia, Tetragonal, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Density | 6.10 g/cc | 0.220 lb/in³ | |
Ferro IP 510 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Density | 6.10 g/cc | 0.220 lb/in³ | |
China Tungsten NT2 Titanium Carbide and Nitride Based Carbides Fine finishing and finishing of steel, cast-irons, Si-AL alloys.Information provided by China Tungsten |