Polymer Property : Density = 6.33 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.33 g/cc
0.229 lb/in³
Ametek P303L P/M Stainless Steel, Sintered from 6.23 g/cc Green Density
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..