Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.70 g/cc | 0.242 lb/in³ | |
Ferro EG 2783 Thick Film Glass Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
Density | 6.70 g/cc | 0.242 lb/in³ | |