Physical Properties Metric English Comments
Density 7.685 g/cc
0.2776 lb/in³
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..
Density 7.685 g/cc
0.2776 lb/in³
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..