Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.96 g/cc | 0.288 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800) AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Density | 7.96 g/cc | 0.288 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700) AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |