Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.03 g/cc | 0.290 lb/in³ | |
IBC Advanced Alloys 10% BeCu Beryllium Copper Master Alloy Beryllium copper “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and n.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
IBC Advanced Alloys 4% BeCu Beryllium Copper Master Alloy Beryllium copper “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and n.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Lucas-Milhaupt Silvaloy® 2M Brazing Alloy Silvaloy 2M is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel LESCALLOY M50 VIM-VAR steel is a through-hardening grade with high hardness and high compressive strength at elevated temperatures. It is produced exclusively as a double vacuum melted produced usi.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Carlson 317L 4 Austenitic Stainless Steel General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Carlson 317L Austenitic Stainless Steel Carlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel and molybdenum prese.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
Carlson 926 Mo Austenitic Stainless Steel General DescriptionCarlson alloy 926 Mo is a “super-austenitic” 6% molybdenum stainless steel that provides excellent resistance to a variety of highly corrosive environments. This alloy performs.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 309H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 309Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 310H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400) Allegheny Ludlum Type 334 is a titanium- and aluminum-bearing austenitic stainless steel offering superior elevated temperature scaling resistance compared to the conventional chromium-nickel stainl.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300) Allegheny Ludlum's 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allvac® Nickelvac® 304 L UNS S30403 Specialty Steel Widely used stainless steel for corrosion resistant application. CPI HX and vessels, tubing, wire, medical and dental devices.Property values are for samples in the metallurgical condition: 1900°F .. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allvac® Vasco® 317 L UNS S31703 Specialty Steel Uses: Turbine components, heat exchangers, pulp & paper equipment, chemical process equipment, semiconductor systems.Property values are for samples in the metallurgical condition: 1900°F anneal.In.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum AL 219 High Strength Specialty Steel Alloy (Alloy 21-6-9), UNS S21904 Property data below is typical of annealed samples. Available in sheet, strip and plate. Intended for high-strength non-magnetic applications and aircraft parts such as hydraulic tubing.Informatio.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Density | 8.03 g/cc | 0.290 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |