Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.20 g/cc | 0.296 lb/in³ | |
Kennametal Stellite Deloro® 40G Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding ach.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® 6 PM cast Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) die.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® 6 PM with P/M Processing Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) die.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 25.4-50.8 mm forged bar, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 1185°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 40% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, GTAW, 9.5 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | at RT |
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 35% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, SMAW, 3.2 mm sheet Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 12.7-50.8 mm hot-rolled bar, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 10% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 20% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 5% Cold Worked, Aged 5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte.. |