Polymer Property : Density = 8.60 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.40 - 8.60 g/cc
0.303 - 0.311 lb/in³
Pacific Sintered Materials CU-143-W Copper Powdered Metal
Applications: High electrical and thermal conductivity. Good for heat sinks and electrical components.All information provided by Pacific Sintered Metals.
Density 8.40 - 8.60 g/cc
0.303 - 0.311 lb/in³
PSM Industries Pacific Sintered Metals Copper CU-143-W Powdered Metal
High electrical and thermal conductivity, Good for heat sinks and electrical problemsInformation Provided by Pacific Sintered Metals, a division of PSM Industries