Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.32 g/cc | 0.337 lb/in³ | |
Indium Corp. Indalloy 43 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.32 g/cc | 0.337 lb/in³ | |
Indium Corp. Indalloy 44 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.32 g/cc | 0.337 lb/in³ | |
Ametek Molybdenum-Copper Composite AMC 3169 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |