Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.39 g/cc | 0.339 lb/in³ | |
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.39 g/cc | 0.339 lb/in³ | |
Indium Corp. Indalloy 134 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.39 g/cc | 0.339 lb/in³ | |
Williams Advanced Alloys WS243 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |