Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 0.500 cc-mm/m²-24hr-atm | 1.27 cc-mil/100 in²-24hr-atm | Average value: 0.500 cc-mm/m²-24hr-atm Grade Count:3 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Nitrogen Transmission | 0.500 cc-mm/m²-24hr-atm | 1.27 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
Nitrogen Transmission | 0.500 cc-mm/m²-24hr-atm | 1.27 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON M-300P PCTFE Pellets NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 0.500 cc-mm/m²-24hr-atm | 1.27 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON M-400H PCTFE Granular Molding Powder NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process.. |