Nitrogen Transmission 59.0 cc-mm/m²-24hr-atm
150 cc-mil/100 in²-24hr-atm
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content
Features: Good mechanical characteristics.Information provided by Daikin Industries.