Chlorine Transmission 0.217 cc-mm/m²-24hr-atm
0.550 cc-mil/100 in²-24hr-atm
23°C
Parylene Coating Services D Poly (P-Xylylene)
Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-par..