Physical Properties Metric English Comments
Kinematic Viscosity 1.23 cSt
1.23 cSt
ASTM D445
ExxonMobil Solvesso™ 150 Aromatic Fluid
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Kinematic Viscosity 1.23 cSt
1.23 cSt
ASTM D445
ExxonMobil Varsol™ 1 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Central America, North America and South AmericaInformation provided by ExxonMobil