Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 1.6 cSt | 1.6 cSt | |
Dow Corning Z-1221 PHENYLMETHYLDICHLOROSILANE Information provided by Dow Corning |
|||
Kinematic Viscosity | 1.6 cSt | 1.6 cSt | |
Dow Corning Z-6011 SILANE Dow Corning® Z-6011 Silane is a reactive chemical containing an aminopropyl organic group and a triethoxysilyl inorganic group. Chemically, Dow Corning® Z-6011 Silane is designated gammaaminopropy.. |