Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 16970 cSt @Temperature -40.0 °C |
16970 cSt @Temperature -40.0 °F |
ASTM D445 |
ExxonMobil Exterex™ A51 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |