Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 1710 cSt @Temperature 50.0 °C |
1710 cSt @Temperature 122 °F |
|
ChevronTexaco Crater® Fluid H Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |