Physical Properties Metric English Comments
Kinematic Viscosity 2.2 cSt
2.2 cSt
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..