Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 2430 cSt @Temperature -40.0 °C |
2430 cSt @Temperature -40.0 °F |
ASTM D445 |
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices.. |