Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 330 cSt @Temperature 25.0 °C |
330 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ TINTM-E Triisononyl Trimellitate Branched C9 trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |