Kinematic Viscosity 392500 cSt

@Temperature -40.0 °C
392500 cSt

@Temperature -40.0 °F
ASTM D445
ExxonMobil Synesstic™ 12 Synthetic Fluid
Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit..