Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 4000 cSt @Temperature 25.0 °C |
4000 cSt @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 294 COATING Syl-Off® 294 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 40 percent solids dispersion of a blend of reactive silox.. |
|||
Kinematic Viscosity | 4000 cSt | 4000 cSt | |
Dow Corning 2-1463 EMULSION Dow Corning 2-1463 Emulsion is a non-ionic emulsion of a gum / cyclic polydimethylsiloxane blend suitable to provide a "Fabric Care" benefit for rinse cycle fabric softeners. The use of this product.. |