Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 50 cSt @Temperature 25.0 °C |
50 cSt @Temperature 77.0 °F |
Base Oil; ASTM D445 |
Nye Lubricants 309 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity | 50 cSt @Temperature 25.0 °C |
50 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ 901P-N Di (Nonyl, Decyl, Undecyl) Phthalate Linear phthalate esterInformation provided by PolyOne |
|||
Kinematic Viscosity | 50 cSt @Temperature 25.0 °C |
50 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ 901P-E Di (Nonyl, Decyl, Undecyl) Phthalate Linear phthalate esterNote: Contains 0.1 - 0.15 wt% 1,1,3-Tris (2-methyl-4-hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |