Polymer Property : Kinematic Viscosity = 5000 cSt
Polymer Property :
Kinematic Viscosity =
5000 cSt
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Kinematic Viscosity
5000
cSt
5000
cSt
Dow Corning 2-9148 RESIN
25% silicone resin in silicone fluid.Information provided by Dow Corning