Polymer Property : Neck In = 1.50 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 3.80 cm
1.50 in
328 ft/min (100 m/min), Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin
Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal..
Neck In 3.81 cm
1.50 in
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 201.48 Low Density Polyethylene Resin
Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal..