Physical Properties Metric English Comments
Neck In 4.30 cm
1.69 in
at 100 m/min, 35rpm, 295°C; ExxonMobil Method
ExxonMobil EXXCO™ Exxco 012 w/40% LDPE Enhanced Performance Extrusion Coating Resin
Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre..