Physical Properties Metric English Comments
Neck In 6.80 cm
2.68 in
BTM 14920
Borealis CA8200 Low Density Polyethylene
CA8200 is a low-density polyethylene for extrusion coating. CA8200 contains no additives. Applications: extrusion coating of high volume production of boards and papers, and coating of various pla..
Neck In 6.80 cm
2.68 in
BTM 14920
Borealis CA7230 Low Density Polyethylene
CA7230 is a low-density polyethylene for extrusion coating. CA7230 contains no additives. Applications: Extrusion coating of high volume production of boards and papers. Coating of various plasti..