Polymer Property : Neck In = 3.30 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 3.30 cm
1.30 in
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin
Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala..