Physical Properties Metric English Comments
Neck In 3.60 cm
1.42 in
164 ft/min (50 m/min), Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LD 200.48 Extrusion Coating and Laminating Resin
Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala..
Neck In 3.60 cm
1.42 in
328 ft/min (100 m/min), Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LD 200.48 Extrusion Coating and Laminating Resin
Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala..
Neck In 3.60 cm
1.42 in
ExxonMobil Method
ExxonMobil LD 202.48 Extrusion Coating Resin
Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro..