Polymer Property : Neck In = 4.80 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 4.80 cm
1.89 in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Dow 4012 Low Density Polyethylene (LDPE)
Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow