Polymer Property : Drawdown = 475 ft/min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Drawdown 2.41 m/s
475 ft/min
at 35 rpm, 295°C; ExxonMobil Method
ExxonMobil EXXCO™ Exxco 012 w/40% LDPE Enhanced Performance Extrusion Coating Resin
Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre..