Physical Properties Metric English Comments
Coating Weight 10.0 g/m²
6.25 lb/ream
BTM 00117
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g..
Coating Weight >= 10.0 g/m²
>= 6.25 lb/ream
BTM 00117
Borealis WG341C Polypropylene
WG341C is a polypropylene for extrusion coating. Applications: microwave oven applications, extrusion coating of high volume production of boards and papers, coating of textile fibers, pinholes fre..