Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Coating Weight = 10.1 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 18MB090 OPP Film
Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM348 OPP Film
Product Description: An enhanced barrier metalized film with a very broad seal range designed to be used in laminate with OPP or Polyester for HFFS applications. The design of this film allows excel..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM383 OPP Film
Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM483 OPP Film
Product Description: A biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance packaging ap..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM488 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM882 OPP Film
Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, ..
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM883 OPP Film
Product Description: An ultra high barrier (UHB), biaxially oriented multilayer polypropylene film. This film has an exceptional barrier to oxygen, flavors and aromas and has an excellent water vapo..