Physical Properties Metric English Comments
Coating Weight 17.4 g/m²
10.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 70 HBS-2 OPP Film
Product Description: Bicor HBS-2 is a one-side sealable, one-side high barrier PVdC-coated OPP film designed for use as the inside sealant web in high-barrier laminations.Availability: Latin America..