Polymer Property : Coating Weight = 112.5 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 112.5 - 132.5 g/m²
70.31 - 82.81 lb/ream
per side
ArcelorMittal Extragal® Z225 Double-sided pure zinc galvanized steel
Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib..